Joint-Braiding |
|
Construction
of Multi-Braiding Composites |
Braiding has the braiding
yarn and middle-end-fiber.
Angle of braiding yarn can be changed from 10 to 80 degree.
The middle-end-fiber keeps always 0 degree.
The braiding layer is maximum 10 layers on our experience. |
 |
|
| One example
to manufacture Joint-Braiding Composite. |
|
 |
| 1st step |
2nd step |
3rd step |
4th step |
5th step |
6th step |
| |
| Advantage of
Joint-Braiding Composite |
-
Seamless, thickness uniformity, fiber
density uniformity
-
Angle of braiding yarn can be controlled
from 10 to 80 degree
-
Multi-node complicated jointing composite
(Max. 10 layers by our experience)
- Various kind of application of joint part
|
Satellite Truss |
Pipe |
 |
  |
|
|
| © Copy right 1996-2005 Murata Machinery
Co.,Ltd. All right reserved. |